Hello all,
We have a gMax 1.5 XT+ dual extrude printer running marlin 1.1.9 and fitted with the gCreate heated bed.
I've been trying to print models with a large base size (anything which falls outside the 8x8" centre zone).
Each time I do some or all the edges of the print start to lift which eventually fouls the part.
I've had the same problem printing in both PLA and ABS.
The heated bed has been set to the recommended temperatures set by the filament manufacturer for each material type and I have tried a number of adhesion additives like a glue stick, blue tape and hair spray.
Are there any tips anyone has to overcome edge lifting?
Photo attached for the sort of thing i'm talking about.
Any and all suggestions will be very welcome.
Cheers,
Ben
We have a gMax 1.5 XT+ dual extrude printer running marlin 1.1.9 and fitted with the gCreate heated bed.
I've been trying to print models with a large base size (anything which falls outside the 8x8" centre zone).
Each time I do some or all the edges of the print start to lift which eventually fouls the part.
I've had the same problem printing in both PLA and ABS.
The heated bed has been set to the recommended temperatures set by the filament manufacturer for each material type and I have tried a number of adhesion additives like a glue stick, blue tape and hair spray.
Are there any tips anyone has to overcome edge lifting?
Photo attached for the sort of thing i'm talking about.
Any and all suggestions will be very welcome.