Hi!
I'm having problems printing XT-CF on my gMax 1.5
Currently Im using the following settings:
Printer itself:
E3D Full metal hotend
0.4mm Nozzle (ruby Nozzle)
Layerhight 0.3mm
10% triangular infill
2 Outlines
3 bottom and top layers
30mm/s default speed
80% underspeed onoutline and solid infill
Temp nozzle 280/260 (have to print about 10 degrees hotter with the Ruby Nozzle)
Bed at 90 degrees
Whats happening is that when the first three layers are printed (prints perfect) and the two outlines are printed on layer 4 it starts skipping on the infill?
Even if I lower speed really low its skipping, and I cant understand why?
PLA seems to print just great! Is the PSU to weak to handle the high temps?
I know that I'm pushing it with the layer height, but I really need perfect layer adhesion, and the object is 500mm tall, so I would really manage to print at 0.3mm layer heights. I've also tested a 0.8mm nozzle at 0.3mm layers, 0.4 and 0.6 mm layers but I cant get rid of the skipping.
Attached the STL file if you want to take a look at it!
https://drive.google.com/open?id=0B21eO ... ndwQ2tDSU0
Im testing 0.2mm layers now, and I cant see any difference, it still skips at 30mm/s:
Swiched to NGEN printing at 250c (0.3mm layers), and that prints fine at 30mm/s and 130% speed (just occasional skipping during infill..)
I'm having problems printing XT-CF on my gMax 1.5
Currently Im using the following settings:
Printer itself:
E3D Full metal hotend
0.4mm Nozzle (ruby Nozzle)
Layerhight 0.3mm
10% triangular infill
2 Outlines
3 bottom and top layers
30mm/s default speed
80% underspeed onoutline and solid infill
Temp nozzle 280/260 (have to print about 10 degrees hotter with the Ruby Nozzle)
Bed at 90 degrees
Whats happening is that when the first three layers are printed (prints perfect) and the two outlines are printed on layer 4 it starts skipping on the infill?
Even if I lower speed really low its skipping, and I cant understand why?
PLA seems to print just great! Is the PSU to weak to handle the high temps?
I know that I'm pushing it with the layer height, but I really need perfect layer adhesion, and the object is 500mm tall, so I would really manage to print at 0.3mm layer heights. I've also tested a 0.8mm nozzle at 0.3mm layers, 0.4 and 0.6 mm layers but I cant get rid of the skipping.
Attached the STL file if you want to take a look at it!
https://drive.google.com/open?id=0B21eO ... ndwQ2tDSU0
Im testing 0.2mm layers now, and I cant see any difference, it still skips at 30mm/s:
Swiched to NGEN printing at 250c (0.3mm layers), and that prints fine at 30mm/s and 130% speed (just occasional skipping during infill..)